Unit | Width | Length | Units per Case | Cases per Pallet | Units per Pallet |
---|---|---|---|---|---|
Roll | 9 in. | 300 ft. | 16 | 8 | 128 |
<b>DuPont™ Tyvek® IntegrationWrap™</b> exhibits physical properties as indicated below when tested as represented. Review all instructions and (Material) Safety Data Sheet ((M)SDS) before use. Please contact DuPont at 1-833-338-7668 when additional guidance is required for writing specifications that include this product.
TEST METHOD | TEST TITLE | PROPERTY | RESULTS |
---|---|---|---|
STRENGTH | |||
ASTM D1777 | Standard Test Method for Thickness of Textile Materials | Thickness | 7 mil |
ASTM F1306 | Standard Test Method for Slow Rate Penetration Resistance of Flexible Barrier Films and Laminates | Puncture Resistance | 20 lbf |
ASTM D882 | Standard Test Method for Tensile Properties of Thin Plastic Sheeting | Tensile Strength | 60/67 MD/CD, lbf |
ASTM D5034 | Standard Test Method for Breaking Strength and Elongation of Textile Fabrics (Grab Test) | Tensile Strength | 95/126 MD/CD, lbf |
ASTM D4533 | Standard Test Method for Trapezoid Tearing Strength of Geotextiles | Tear Resistance | 22/37 MD/CD, lbf |
AIR | |||
TAPPI T-460 | Air resistance of paper (Gurley method), Test Method | Material Air Resistance | > 10,000 sec/100 cc |
ASTM E1677 | Standard Specification for Air Barrier (AB) Material or Assemblies for Low-Rise Framed Building Walls | Assembly Air Leakage | < 0.04 cfm/ft2 (0.2 L/s • m2) |
WATER | |||
ASTM E96 | Standard Test Methods for Gravimetric Determination of Water Vapor Transmission Rate of Materials | Water Vapor Transmission Method A (Dry Cup) & Method B (Wet Cup) | < 1 perms |
ASTM E331 | Standard Test Method for Water Penetration of Exterior Windows, Skylights, Doors, and Curtain Walls by Uniform Static Air Pressure Difference | Assembly Water Resistance | 300 Pa 6.24 psf |
AATCC 127 | Test Method for Water Resistance: Hydrostatic Pressure | Material Water Resistance (Dynamic Method) | > 500 cm water column |
AATCC 127 | Test Method for Water Resistance: Hydrostatic Pressure | Hydrostatic Head Pressure (Static Method) | PASS 55 cm for 24 hours |
GENERAL | |||
ASTM G154 | Standard Practice for Operating Fluorescent Ultraviolet (UV) Lamp Apparatus for Exposure of Non-Metallic Materials | Ultra-Violet Light (UV) Exposure Limit | 120 days |
AAMA 712 | Voluntary Specification for Mechanically Attached Flexible Flashing | Passes full AAMA 712 | PASS |
Note:- *Tyvek® IntegrationWrap™ tested in a wall assembly containing a window. In accordance with the DuPont™ Tyvek® IntegrationWrap™ Installation Guidelines, DuPont Self-Adhered Flashing Products were used to flash window to Tyvek® IntegrationWrap™, with Tyvek® IntegrationWrap™ sealed to Tyvek® WRB on the wall using DuPont™ Tyvek® Tape.